Introduction To Haynes Superalloys 160 / UNS N07160

Haynes-160

MOKSH TUBES & FITTINGS LLP is a leading manufacturer, supplier, exporter, importer, and stockist of a broad range of Haynes 160 (UNS N07160) products. including Pipes & Tubes, Pipe Fittings, Flanges, Fasteners, Sheets & Plates, Coils, Wires, Round Bars, Flat Bars, Angles, Channels, Welding Rods, Wire Mesh, and other custom and hard-to-find Haynes 160 products.

Haynes Superalloys 160 is a nickel-chromium-iron alloy known for its excellent resistance to oxidation and carburization in highly aggressive environments. It offers outstanding high-temperature strength and corrosion resistance, making it an ideal choice for demanding industrial applications.

Chemical Composition

Element Composition (%)
Nickel Balance
Chromium 22.0 – 24.0
Iron 17.0 – 20.0
Manganese ≤ 1.0
Silicon ≤ 0.35
Carbon ≤ 0.10
Aluminum ≤ 0.30
Titanium ≤ 0.30
Phosphorus ≤ 0.015
Sulfur ≤ 0.015

Technical Composition

Physical Properties

Property Imperial Metric
Density 0.304 lb/in³ 8.43 g/cm³
Melting Point 2560–2700 °F 1404–1482 °C
Specific Heat 0.12 Btu/lb·°F 502 J/kg·°C
Curie Temperature
Magnetic Permeability at 200 oersteds (15.9 kA/m) 1.02

Mechanical Properties

Property Plate (Annealed) Bar/Rod (Annealed) Sheet (Annealed) Tube/Cold‑drawn
Tensile Strength (ksi / MPa) 112 ksi / 774 MPa 111 ksi / 767 MPa 110 ksi / 758 MPa 111 ksi / 767 MPa
Yield Strength (0.2%) (ksi / MPa) 46 ksi / 321 MPa 45 ksi / 314 MPa 51 ksi / 353 MPa 45 ksi / 314 MPa
Elongation (%) 66 % 68 % 63–68 % 68 %
Reduction of Area (%) 73 %
Modulus of Elasticity (GPa) 211 GPa 211 GPa sheet same as plate

Products in Haynes Superalloys 160

Haynes Superalloys 160 is offered in numerous product forms meeting ASTM, ASME, and other standards:

Seamless Pipes
Welded Pipes (ERW & EFW)
Tubes (Capillary, U-Bend)
Sheets & Plates
Coils & Strips
Round Bars, Flat Bars, Hex Bars, Square Bars
Pipe Fittings (Elbows, Tees, Reducers, Caps, Stub Ends)
Flanges (Weld Neck, Slip-On, Blind, Socket Weld, Threaded)
Fasteners (Bolts, Nuts, Screws, Washers, Studs)
Custom Fabricated Components

Haynes Superalloys 160 products are produced to the following global standards:

Uses and Advantages

Excellent oxidation and carburization resistance up to 1100°C (2000°F)
Strong high-temperature strength and durability
Outstanding corrosion resistance in oxidizing and reducing environments
Good fabricability and weldability
Resistance to thermal fatigue and creep

Applications of Haynes Superalloys 160

Haynes Superalloys 160 Commonly used in industries requiring reliable performance under extreme conditions:

Aerospace Industry

Components exposed to high temperatures such as combustion chambers and heat shields

Industrial Furnaces and Heat Treating

Parts subjected to continuous high temperatures and aggressive atmospheres

Chemical Processing

Reactors, vessels, and piping exposed to corrosive chemicals

Power Generation

Gas turbine components and boiler parts

Environmental Control

Equipment handling flue gas and exhaust streams

WHY CHOOSE US?

Extensive expertise in delivering high-quality nickel alloys
Global sourcing of premium raw materials
Strict quality assurance for consistent product performance
Custom manufacturing to meet specific project needs
Dedicated customer support and technical guidance

FAQ's

What is Haynes 160 and why is it important in high-temperature industries?

Haynes 160 (UNS N07160) is a nickel chromium iron superalloy designed for excellent resistance to oxidation and carburization in aggressive environments. It combines outstanding high temperature strength, durability, and corrosion resistance, making it widely used in industries that operate under extreme thermal and chemical conditions. Its ability to resist thermal fatigue and creep makes it an ideal choice for aerospace, power generation, chemical processing, and furnace applications.

What are the main properties of Haynes 160 alloy?

Haynes 160 offers excellent mechanical and thermal properties with a tensile strength of around 112 ksi, yield strength of 46 ksi, and elongation of up to 68%. It has a density of 8.43 g/cm³, a melting point between 1404–1482°C, and provides resistance to oxidation and carburization up to 1100°C (2000°F). Along with superior fabricability and weldability, this alloy ensures long term stability and performance under harsh operating conditions.

Which industries commonly use Haynes 160 products?

Haynes 160 is extensively used in aerospace for high-temperature components such as combustion chambers and heat shields, in industrial furnaces and heat treating equipment for burner parts and retorts, and in chemical processing for reactors, vessels, and piping that handle corrosive media. It also plays a crucial role in power generation for gas turbine parts and boiler components, as well as in environmental control systems that manage flue gas and exhaust streams.

What types of Haynes 160 products are available from MOKSH TUBES & FITTINGS LLP?

MOKSH TUBES & FITTINGS LLP offers a complete range of Haynes 160 products including seamless and welded pipes, tubes, sheets, plates, coils, bars, flanges, pipe fittings, fasteners, wire mesh, welding rods, and custom-fabricated components. All products are manufactured in compliance with ASTM, ASME, and other international standards, ensuring superior quality and long-lasting performance for critical industrial applications.

Why choose MOKSH TUBES & FITTINGS LLP for Haynes 160 materials?

MOKSH TUBES & FITTINGS LLP is a leading global supplier with extensive expertise in nickel based superalloys like Haynes 160. The company ensures premium quality through strict quality assurance, global sourcing of raw materials, and adherence to international standards. With custom manufacturing options, timely delivery, and dedicated technical support, MOKSH TUBES & FITTINGS LLP provides reliable solutions that meet the demands of industries operating under extreme conditions.

Contact Us

Moksh Tubes & Fittings LLP your dependable partner for specialty alloys.

Get in Touch