Introduction To Haynes Superalloys 188 / UNS N06188

Haynes-188

MOKSH TUBES & FITTINGS LLP is a manufacturer, supplier, exporter, importer, and stockist of a wide range of Haynes 188 (UNS N06188) products. Including Pipes & Tubes, Pipe Fittings, Flanges, Fasteners, Sheets & Plates, Coils, Wires, Round Bars, Flat Bars, Angles, Channels, Welding Rods, Wire Mesh, and other custom and hard-to-find Haynes 188 products.

Haynes Superalloys 188 is a cobalt-based superalloy known for its excellent strength, corrosion resistance, and exceptional resistance to oxidation and carburization at high temperatures. It is widely used in aggressive high-temperature environments, especially where resistance to thermal fatigue and creep is critical.

Chemical Composition

Element Composition (%)
Cobalt Balance
Chromium 22.0 – 24.0
Nickel 14.5 – 16.5
Molybdenum 4.0 – 5.0
Iron ≤ 2.0
Manganese ≤ 1.0
Silicon ≤ 0.35
Carbon ≤ 0.10
Aluminum ≤ 0.30
Titanium ≤ 0.30
Phosphorus ≤ 0.015
Sulfur ≤ 0.015

Technical Composition

Physical Properties

Property Imperial Metric
Density 0.302 lb/in³ 8.36 g/cm³
Melting Point 2475–2650 °F 1357–1454 °C
Specific Heat 0.11 Btu/lb·°F 460 J/kg·°C
Curie Temperature
Magnetic Permeability at 200 oersteds (15.9 kA/m) 1.02

Mechanical Properties

Property Tubing (Annealed) Tubing (Cold Drawn) Bar (Annealed) Plate (Annealed) Sheet (Annealed)
Tensile Strength (ksi) 143 150 125 (min) 144 142
Tensile Strength (MPa) 986 1034 862 (min) 991 982
Yield Strength (0.2%) (ksi) 70 75 55 (min) 70 70
Yield Strength (MPa) 483 517 379 (min) 483 483
Elongation (%) 50 45 45 (min) 50.6 50.9

Products in Haynes Superalloys 188

Haynes Superalloys 188 is available in a variety of forms, complying with ASTM, ASME, and other standards:

Seamless Pipes
Welded Pipes (ERW & EFW)
Tubes (Capillary, U-Bend)
Sheets & Plates
Coils & Strips
Round Bars, Flat Bars, Hex Bars, Square Bars
Pipe Fittings (Elbows, Tees, Reducers, Caps, Stub Ends)
Flanges (Weld Neck, Slip-On, Blind, Socket Weld, Threaded)
Fasteners (Bolts, Nuts, Screws, Washers, Studs)
Custom Fabricated Components

Haynes Superalloys 188 products are produced to the following global standards:

Uses and Advantages

Exceptional high-temperature strength and creep resistance
Superior oxidation and carburization resistance up to ~1093 °C (2000 °F)
Excellent thermal fatigue resistance
Good fabricability and weldability
Stability in harsh corrosive and oxidizing environments

Applications of Haynes Superalloys 188

Haynes Superalloys 188 Widely used in industries requiring high-performance alloys under severe conditions:

Aerospace and Gas Turbine Components

Combustion chambers, turbine blades, hot section components

Industrial Furnaces and Heat Treating Equipment

Furnace parts exposed to extreme temperatures

Chemical Processing

Reactors and heat exchangers in corrosive environments

Power Generation

Components in steam turbines and boilers

Environmental Control Equipment

Parts for incinerators and flue gas treatment

WHY CHOOSE US?

Extensive experience in manufacturing and supplying cobalt-based superalloys
Strict quality controls ensuring compliance with industry standards
Wide global supply chain for on-time delivery
Customized product solutions and expert technical support
Dedicated customer support and technical guidance

FAQ's

What is Haynes 188 and why is it used in high-temperature applications?

Haynes 188 (UNS N06188) is a cobalt-based superalloy well known for its exceptional strength, corrosion resistance, and remarkable resistance to oxidation and carburization at elevated temperatures. It performs reliably in aggressive environments where components are exposed to extreme heat and stress, making it one of the most trusted alloys in aerospace, chemical processing, and power generation industries.

What are the key properties of Haynes 188 alloy?

Haynes 188 exhibits superior high-temperature strength, creep resistance, and stability in harsh conditions. It offers a tensile strength of up to 150 ksi, yield strength of 70 ksi, and elongation of around 50%. With excellent resistance to oxidation and carburization up to 2000°F (1093°C), combined with good thermal fatigue resistance, fabricability, and weldability, this alloy provides long-lasting performance in demanding applications.

Which industries commonly use Haynes 188 products?

Haynes 188 is widely used in aerospace for gas turbine components such as combustion chambers, hot section parts, and turbine blades, in industrial furnaces for heat-treating equipment, in chemical processing for reactors and heat exchangers handling corrosive media, and in power generation for steam turbine and boiler parts. It is also applied in environmental control equipment such as incinerators and flue gas treatment systems due to its ability to withstand aggressive thermal and chemical conditions.

What types of Haynes 188 products are available from MOKSH TUBES & FITTINGS LLP?

MOKSH TUBES & FITTINGS LLP supplies a complete range of Haynes 188 products including seamless and welded pipes, tubes, sheets, plates, coils, bars, flanges, pipe fittings, fasteners, welding rods, wire mesh, and custom fabricated components. All materials are produced according to ASTM, ASME, and other international standards, ensuring superior quality, consistency, and performance for critical industrial applications.

Why choose MOKSH TUBES & FITTINGS LLP for Haynes 188 materials?

MOKSH TUBES & FITTINGS LLP is a trusted manufacturer and global supplier of cobalt based superalloys like Haynes 188, offering expertise, strict quality assurance, and a robust supply chain. With a focus on custom manufacturing, technical support, and timely delivery, the company ensures clients receive high performance materials that meet industry standards and project requirements, making it a reliable partner for industries operating in extreme environments.

Contact Us

Moksh Tubes & Fittings LLP your trusted partner in specialty alloys.

Get in Touch