Introduction To Nickel 200 / Alloy 200 / UNS N02200

Nickel 200

MOKSH TUBES & FITTINGS LLP is a trusted manufacturer, supplier, exporter, importer, and stockist of a wide range of NICKEL 200 products including Pipes & Tubes, Pipe Fittings, Flanges, Fasteners, Sheets & Plates, Coils, Wires, Round Bars, Flat Bars, Angles, Channels, Welding Rods, Wire Mesh, and other Custom and Hard-to-Find Nickel 200 Components.

Nickel 200, is a commercially pure wrought nickel alloy (99.6% Ni) that offers excellent resistance to a wide range of corrosive environments. It exhibits outstanding mechanical properties and exceptional resistance to alkaline media, especially in caustic soda and other strongly alkaline solutions. This solid-solution strengthened alloy is highly ductile, making it ideal for both hot and cold working, and is particularly suited for applications requiring high thermal and electrical conductivity.

Chemical Composition

Element Composition (%)
Nickel 99.0
Copper 0.25 max
Iron 0.40 max
Manganese 0.35 max
Silicon 0.35 max
Carbon 0.15 max
Sulfur 0.01 max

Technical Composition

Physical Properties

Property Imperial Metric
Density 0.321 lb/in³ 8.89 g/cm³
Melting Range 2615 – 2635 °F 1435 – 1446 °C
Specific Heat 0.109 Btu/lb•°F 456 J/kg•°C
Curie Temperature 680 °F 360 °C

Mechanical Properties

Property Rod and Bar (Hot-Finished) Rod and Bar (Cold-Drawn) Rod and Bar (CD Annealed or HF Annealed) Plate (Hot-Rolled) Plate (Hot-Rolled Annealed) Sheet (Hard) Sheet (Annealed) Strip (Spring) Strip (Annealed) Tubing (Stress-Relieved) Tubing (Annealed) Cond. & Evap. Tubing (Annealed) Cond. & Evap. Tubing (Stress-Relieved) Wire (Annealed) Wire (No. 1 Temper) Wire (Spring Temper)
Brinell Hardness (MP 3000 kg) 60–85 65–110 55–75 55–100 55–80 90–115 55–75 90–130 55–75 65–110 55–75 55–75 65–110 55–85 70–95 125–145
Yield Strength (ksi) 15–45 40–100 15–30 20–80 15–40 70–105 15–30 70–115 15–30 40–90 12–30 15–30 40–90 15–50 40–75 105–135
Yield Strength (MPa) 105–310 275–690 105–210 140–550 105–275 480–725 105–210 480–795 105–210 275–620 85–210 105–210 275–620 105–345 275–520 725–930
Tensile Strength (ksi) 55–35 35–10 55–40 55–35 60–40 15–2 55–40 15–2 55–40 35–15 60–40 60–40 35–20 50–30 40–20 15–2
Elongation % (in 2 in/51 mm) 90–150 140–230 90–120 100–150 90–140

Products in NICKEL 200

NICKEL 200 (UNS N02200 / W.Nr. 2.4066) is known for its purity and resistance to alkaline environments. It is widely used in electrical, chemical, and food processing applications due to its ability to resist corrosion and maintain strength in extreme environments.

Seamless Pipes
Welded Pipes (ERW & EFW)
Tubes (Capillary, U-Bend)
Sheets & Plates
Coils & Strips
Round Bars, Flat Bars, Hex Bars, Square Bars
Pipe Fittings (Elbows, Tees, Reducers, Caps, Stub Ends)
Flanges (Weld Neck, Slip-On, Blind, Socket Weld, Threaded)
Fasteners (Bolts, Nuts, Screws, Washers, Studs)
Custom Fabricated Components

This alloy meets several recognized industry standards, including:

Uses and Advantages

Excellent corrosion resistance in caustic and alkaline environments
High thermal and electrical conductivity
Suitable for food processing and handling due to high purity
Outstanding ductility and mechanical strength
Resistant to neutral and alkaline salt solutions
Easy to fabricate and weld using conventional techniques

Applications of Nickel 200

Nickel 200 is a preferred material in industries where purity, resistance to alkalis, and non-magnetic properties are critical. Typical applications include:

Chemical Processing

Used in tanks, vessels, and piping for caustic soda, caustic potash, and chlor-alkali production.

Electronics & Electrical

Ideal for battery components, electrical contacts, terminals, and lead wires due to its conductivity.

Food Processing

Used in handling of fatty acids, fruits, and caustic cleaning solutions.

Aerospace & Defense

Deployed in precision instrumentation and radar/electronics components.

Marine & Offshore

Corrosion-resistant fasteners and components exposed to seawater and saline atmospheres.

Heat Exchangers

Preferred in systems requiring purity and thermal conductivity under caustic conditions.

Medical Equipment

Used in equipment requiring non-reactive and clean-contact materials.

WHY CHOOSE US?

Decades of experience in supplying high-performance nickel alloys
Wide inventory and fast delivery on Nickel 200 materials
Advanced testing and quality assurance protocols
Custom machining and cutting services available
Global network for sourcing and logistics

FAQ's

What is Nickel 200 and what makes it unique?

Nickel 200 (UNS N02200) is a commercially pure wrought nickel alloy containing about 99.6% nickel. It is widely recognized for its excellent resistance to alkaline and caustic environments, outstanding ductility, and high thermal and electrical conductivity. These properties make Nickel 200 an ideal choice for applications requiring both purity and performance, such as chemical processing, food handling, electronics, and marine engineering.

What types of Nickel 200 products does Moksh Tubes & Fittings LLP offer?

Moksh Tubes & Fittings LLP manufactures, supplies, and exports a wide range of Nickel 200 products including seamless and welded pipes, tubes, sheets, plates, coils, wire mesh, round bars, flat bars, angles, channels, flanges, pipe fittings, fasteners, welding rods, and custom-fabricated components. All products meet global industry standards and can be customized to meet specific client requirements across diverse industries.

What are the key benefits of using Nickel 200 in industrial applications?

The main advantages of Nickel 200 include excellent corrosion resistance in caustic and alkaline environments, superior thermal and electrical conductivity, high purity that makes it suitable for food and pharmaceutical industries, and outstanding ductility that allows easy fabrication and welding. Additionally, its non-magnetic properties and mechanical strength make it a reliable material for high-performance applications in aerospace, marine, and power generation.

Which industries commonly use Nickel 200 alloy products?

Nickel 200 is widely used in industries such as chemical processing, food processing, electronics, aerospace, defense, marine, medical, and power generation. It is commonly applied in equipment like tanks, vessels, heat exchangers, piping systems, battery components, electrical contacts, caustic soda production systems, marine fasteners, instrumentation, and medical equipment where purity, durability, and corrosion resistance are critical.

Why choose Moksh Tubes & Fittings LLP for Nickel 200 supply?

Moksh Tubes & Fittings LLP is a trusted global supplier of Nickel 200 products, known for its extensive inventory, ISO certified operations, and commitment to quality assurance. With decades of expertise, advanced testing facilities, and precision machining services, the company ensures reliable supply and timely delivery of Nickel 200 materials. Their dedication to traceability, customer satisfaction, and customized solutions makes them a preferred partner for clients across industries worldwide.

Contact Us

Reach out to Moksh Tubes & Fittings LLP your reliable partner for premium nickel alloy products.

Get in Touch