MOKSH TUBES & FITTINGS LLP is a leading manufacturer, supplier, exporter, importer, and stockist of NICKEL 201 products, offering Pipes & Tubes, Pipe Fittings, Flanges, Fasteners, Sheets, Plates, Coils, Wires, Round Bars, Flat Bars, Angles, Channels, Welding Rods, Wire Mesh, and other customized and specialty Nickel 201 components.
Nickel 201, is a low-carbon version of commercially pure wrought nickel (99.6% Ni), designed to provide enhanced resistance to graphitization in high-temperature environments. It retains the excellent corrosion resistance, thermal and electrical conductivity, and workability of Nickel 200 while offering superior performance in applications above 600 °F (315 °C). The reduced carbon content (0.02% max) minimizes carbide precipitation and ensures resistance to intergranular attack—making Nickel 201 ideal for caustic, food-grade, and high-temperature service environments.
| Element | Composition (%) |
|---|---|
| Nickel | 99.0 |
| Copper | 0.25 max |
| Iron | 0.40 max |
| Manganese | 0.35 max |
| Silicon | 0.35 max |
| Carbon | 0.02 max |
| Sulfur | 0.01 max |
| Property | Imperial | Metric |
|---|---|---|
| Density | 0.321 lb/in³ | 8.89 g/cm³ |
| Melting Range | 2615 – 2635 °F | 1435 – 1446 °C |
| Specific Heat | 0.108 Btu/lb•°F | 450 J/kg•°C |
| Thermal Conductivity | 49.9 W/m·K | 346 BTU·in/hr·ft²·°F |
| Electrical Conductivity | 22% IACS | — |
| Magnetic Permeability | 1.0004 | — |
| Property | Rod & Bar (Hot-Finished / Annealed) | Rod & Bar (Cold-Drawn) | Rod & Bar (Cold-Drawn & Annealed) | Plate (Hot-Rolled) | Plate (Hot-Rolled, Annealed) | Tube/Pipe (Cold-Drawn, Annealed) | Tube/Pipe (Stress-Relieved) |
|---|---|---|---|---|---|---|---|
| Tensile Strength (ksi) | 50–60 | 60–100 | 50–60 | 50–70 | 50–70 | 50–70 | 60–105 |
| Tensile Strength (MPa) | 345–415 | 415–690 | 345–415 | 345–485 | 345–485 | 345–485 | 415–724 |
| Yield Strength (ksi) | 10–25 | 35–90 | 10–25 | 12–35 | 12–35 | 10–28 | 30–85 |
| Yield Strength (MPa) | 70–170 | 240–620 | 70–170 | 83–240 | 83–240 | 70–195 | 207–586 |
| Elongation % | 60–40 | 35–10 | 60–40 | 60–35 | 60–40 | 60–40 | 35–15 |
| Hardness (Brinell / Rockwell) | 75–100 BHN | 125–200 BHN | 75–100 BHN/td> | – | – | ≤ 62 HRB | 70–95 HRB |
NICKEL 201 (UNS N02201 / W.Nr. 2.4068) is a dependable material used across industries requiring purity, excellent ductility, and resistance to alkalis, acids, and elevated temperatures. It performs especially well in processes where Nickel 200’s higher carbon content might lead to embrittlement.
This alloy meets several recognized industry standards, including:
Nickel 201 is trusted in industries that require high chemical resistance and reliability in elevated temperature or purity-demanding environments.
Used in reactors, piping, storage vessels, and caustic solution handling equipment.
Ideal for components like battery connections, terminals, and leads.
Used in caustic wash systems, food-grade tanks, and conveying equipment.
Critical in radar, avionics, and EMI-sensitive shielding applications.
Deployed in caustic and acidic media at elevated service temperatures.
Used in saltwater desalination and anti-corrosive structural components.
Used in reactor vessels, chemical recovery systems, and thermal insulation.
Nickel 201, also known as UNS N02201 or W.Nr. 2.4068, is a low-carbon version of commercially pure wrought nickel (99.6% Ni). Compared to Nickel 200, it offers enhanced resistance to graphitization at high temperatures due to its reduced carbon content (0.02% max), minimizing carbide precipitation and intergranular corrosion. It retains excellent corrosion resistance, thermal and electrical conductivity, and workability, making it suitable for caustic, food-grade, and elevated-temperature applications.
Moksh Tubes & Fittings LLP manufactures, stocks, and exports a wide range of Nickel 201 products including seamless and welded pipes, tubes, sheets, plates, coils, strips, round bars, flat bars, hex bars, square bars, pipe fittings, flanges, fasteners, wires, welding rods, wire mesh, and custom fabricated components. All products are designed to meet high-performance and industrial application requirements.
Nickel 201 provides exceptional resistance to caustic alkalis, acids, and high temperature environments. It is non magnetic, maintains high electrical conductivity, and has excellent mechanical properties and workability. The low carbon content prevents embrittlement and intergranular corrosion, ensuring long term durability and reliability in demanding industrial processes.
Nickel 201 is widely used in chemical and petrochemical industries for reactors, piping, and caustic solution handling equipment; in electronics and battery components; in food processing for caustic wash systems and tanks; in aerospace and defense for EMI-sensitive shielding; in heat exchangers for caustic and acidic media; in marine and offshore for saltwater applications; and in nuclear and power generation for reactor vessels and thermal insulation.
Moksh Tubes & Fittings LLP specializes in high purity nickel alloys with superior corrosion resistance and dimensional accuracy. The company offers ready stock of Nickel 201 in standard and custom sizes, testing and certification according to international norms, fast delivery, precision cutting, and custom fabrication. With global export capabilities and a focus on quality and reliability, they provide dependable solutions for critical industrial applications.
Moksh Tubes & Fittings LLP for reliable, cost-effective, and globally shipped solutions.